Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.800 GPa | 551.1 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0334G25M5CL Glass/Mineral Reinforced Coupled |
|||
Tensile Modulus | 3.800 GPa | 551.1 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0336W40L Wollastonite Reinforced |