Mechanical Properties Metric English Comments
Tensile Modulus 3.45 - 3.79 GPa
500 - 550 ksi
Master Bond EP62-1Med USP Class VI Two Component Epoxy Resin System
Master Bond EP62-1Med is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a 100 to 10 mi..
Tensile Modulus 3.45 - 3.79 GPa
500 - 550 ksi
Master Bond Supreme 10AOHT-LO High Shear and Peel Strength Epoxy
Description: Master Bond Supreme 10AOHT-LO has a combination of properties consisting of excellent thermal conductivity, superior electrical insulation, great adhesion to a wide variety of substrate..