Mechanical Properties Metric English Comments
Tensile Modulus 55.0 GPa
7980 ksi
ASTM D638
Quantum Composites AMC™ 8590 BK 53% Carbon Fiber Reinforced Vinyl Ester SMC
AMC™ 8590 BK is a vinyl ester, chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant,..