Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.94 GPa | 862 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP AF004L ABS LNP* THERMOCOMP* AF004L is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Low Extractible. |
|||
Tensile Modulus | 5.94 GPa | 862 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF003ES PA 66 LNP* THERMOCOMP* RF003ES is a Nylon 66 base resin containing 15% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Tensile Modulus | 5.94 GPa | 862 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF004 PC LNP* THERMOCOMP* DF004 is a compound based on Polycarbonate resin containing 20% Glass Fiber. |