Mechanical Properties Metric English Comments
Tensile Modulus 5.84 GPa
847 ksi
1mm/min; ISO 527
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned)
Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also..
Tensile Modulus 5.84 GPa
847 ksi
same value from ASTM and ISO test.
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron 8233G is a 33% glass fiber reinforced polyamide 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also available in he..