Mechanical Properties Metric English Comments
Tensile Modulus 5.08 GPa
737 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Lubricomp KFL22 Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KFL22 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f..
Tensile Modulus 5.08 GPa
737 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Lubricomp KFL22 Acetal Copolymer
LNP* Lubricomp* KFL22 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f..
Tensile Modulus 5.08 GPa
737 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF002XXH PA 66
LNP THERMOCOMP* RF002XXH is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added feature of this material includes: Healthcare.