Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 34.44 GPa | 4995 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP UX04509 PPA LNP* Thermocomp* UX04509 is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |