Mechanical Properties Metric English Comments
Tensile Modulus 3.43 GPa
498 ksi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® HN-3104 PC, 10% Glass Filled FR
Information provided by Samsung Cheil Industries.
Tensile Modulus 3.43 GPa
498 ksi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® HN-3104 PC, 10% Glass Filled FR
Information provided by Samsung Cheil Industries.