Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 330 GPa | 47900 ksi | Young's; DINV ENV 843-2 |
CeramTec Rubalit® IS 95 Alumina Rubalit® IS 95 is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at eleva.. |
|||
Tensile Modulus | 330 GPa | 47900 ksi | Young's; DINV ENV 843-2 |
CeramTec Rubalit® A 1896 Alumina Rubalit® A 1896 (96%) is an aluminum oxide ceramic with an optimum price/performance ratio. Its outstanding properties are low density, low weight, high corrosion and wear resistance, excellent ele.. |