Polymer Property : Tensile Modulus = 460.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.172 GPa
460.1 ksi
ASTM D638
Resirene Resirene® HH-103 General Purpose Polystyrene
Features:Low FlowHigh HeatHigh Molecular WeightMechanical StrengthFDA Rating: 21 CFR 177.1640Applications:ExtrusionFoamGPPS/HIPS BlendsInformation provided by US distributor Calsak Corporation.