Polymer Property : Tensile Modulus = 4427 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 30.52 GPa
4427 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK
LNP* THERMOCOMP* LC008E is a compound based on Polyetheretherketone resin containing 40% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive.
Tensile Modulus 30.52 GPa
4427 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK (Asia Pacific)
LNP* Thermocomp* LC008E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive.
Tensile Modulus 30.52 GPa
4427 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP EC006APQ PEI
LNP* Thermocomp EC006APQ is a compound based on Polyetherimide containing 30% Carbon Fiber. Added features include: Electrically Conductive, High Flow.