Tensile Modulus 300 GPa
43500 ksi
Young's; DINV ENV 843-2
CeramTec Rubalit® IS 95 Brown Alumina
Rubalit® IS 95 brown is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at..