Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 29.6 GPa | 4300 ksi | RT, Dry, 0° Direction |
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ Astroquartz 4581 Fabric MVK-14 Polyimide Astroquartz and S2 glass prepregs are an affordable, easy-to-process material for high-temperature radome and antenna applications. MVK-14 is a non-MDA alternative to BMI, cyanate e.. |
|||
Tensile Modulus | 29.6 GPa | 4300 ksi | RT, Dry, 0° Direction |
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ S2-Glass Fabric MVK-14 Polyimide Astroquartz and S2 glass prepregs are an affordable, easy-to-process material for high-temperature radome and antenna applications. MVK-14 is a non-MDA alternative to BMI, cyanate e.. |