Mechanical Properties Metric English Comments
Tensile Modulus 0.295 GPa
42.8 ksi
ISO 527-1/-2
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl..
Tensile Modulus 0.295 GPa

@Temperature 120 °C
42.8 ksi

@Temperature 248 °F
ISO Data
BASF Ultramid® 8253 PA6 (Dry)
Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o..