Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 28.6 GPa | 4150 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP OCF62 PPS - Branched LNP* THERMOCOMP* OCF62 is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding |
|||
Tensile Modulus | 28.6 GPa | 4150 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP OCF62E PPS - Branched LNP* THERMOCOMP* OCF62E is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding |