Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 41.379 GPa | 6001.5 ksi | ASTM D-638 |
PlastiComp Complet® LCF50 - PA66 MT Nylon 66, 50% Long Carbon Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementImpact modifiedInformation provided by Pla.. |