Tensile Modulus 279 GPa
40500 ksi
Typical fiber property; Chord 6000-1000
Hexcel® HexTow™ IM6 Carbon Fiber
HexTow™ IM6 carbon fiber is a continuous, high performance, intermediate modulus, PAN based fiber available in 12,000 (12K) filament count tows. The fiber has been surface treated and can be sized ..