Mechanical Properties Metric English Comments
Tensile Modulus 4.943 GPa

@Temperature 23.0 °C
716.9 ksi

@Temperature 73.4 °F
EN ISO 527
Ensinger TECASINT 4021 Polyimide, Black, 15% Graphite (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..