Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.94 GPa | 716 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Tensile Modulus | 4.94 GPa | 716 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP (Asia Pacific) LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact. |