Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.91 GPa | 712 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP ZX05506 PPE+PS LNP LUBRICOMP* ZX05506 is a compound based on PPE+PS Blend resin containing Graphite Powder, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 4.91 GPa | 712 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP ZX05506 PPE+PS (Asia Pacific) LNP LUBRICOMP* ZX05506 is a compound based on PPE+PS Blend resin containing Graphite Powder, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 4.91 GPa | 712 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KFI12 Acetal Copolymer LNP LUBRICOMP* KFI12 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 2% Silicone. Added feature of this grade is: Wear Resistant. |