Polymer Property : Tensile Modulus = 4.699 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 4.699 GPa
681.6 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0334G40CL Glass Reinforced Coupled