Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.304 GPa | 624.3 ksi | UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97) |
CRP Technology Windform® GF 2.0 Polyamide-Aluminum-Glass Composite Processed by selective laser sintering (SLS). Windform® GF 2.0 is the evolutionary substitute for Windform GF, our first generation material. Windform® GF 2.0 is a composite material made of poly.. |