Tensile Modulus 4.238 GPa
614.7 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® CY-10GF/000 UV FR V0 NATURAL PC/ABS Blend, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedNon-HalogenatedFlame RetardantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.