Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.015 GPa @Temperature 120 °C |
582.3 ksi @Temperature 248 °F |
ISO Data |
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Dry) Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature
performance and .. |