Polymer Property : Tensile Modulus = 390 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 390 GPa
56600 ksi
Young's; DINV ENV 843-2
CeramTec V 679 Alumina, 99.7%
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.
Tensile Modulus 390 GPa
56600 ksi
Young's; DINV ENV 843-2
CeramTec AT 79 Alumina, 99.6%
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.