Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.584 GPa | 374.8 ksi | ISO 527-1,2 |
Nanocyl PLASTICYL™ PC1501 Polycarbonate with 2 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |