Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 25.7 GPa | 3730 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP 9X06030 PA 46 (Europe-Africa-Middle East) LNP* LUBRICOMP* 9X06030 is a compound based on PA46 resin containing PTFE and Carbon Fiber. Added features include: Internally Lubricated, Heat Stabilized. |