Polymer Property : Tensile Modulus = 365.2 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.518 GPa
365.2 ksi
ASTM D638
Ashley Polymers Ashlene® ABS Resin E213B
General purpose, black, utility grade for injection molding with medium gloss.Data provided by the manufacturer