Mechanical Properties Metric English Comments
Tensile Modulus 0.249 GPa
36.1 ksi
ISO 527
Lubrizol ESTANE® GP65DE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 65DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..