Mechanical Properties Metric English Comments
Tensile Modulus 24.56 GPa
3562 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp LC006E PEEK
LNP THERMOCOMP* LC006E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Am..