Polymer Property : Tensile Modulus = 35.48 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 35.48 GPa
5146 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP EC008APQ PEI
LNP* THERMOCOMP* EC008APQ is a compound based on Polyetherimide containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, High Flow.
Tensile Modulus 35.48 GPa
5146 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP EC008PXQ PEI
LNP* THERMOCOMP* EC008PXQ is a compound based on Polyetherimide containing 40% Carbon FIber. Added features include: Electrically Conductive, Exceptional Processing