Mechanical Properties Metric English Comments
Tensile Modulus 2.38 GPa

@Thickness 3.20 mm
346 ksi

@Thickness 0.126 in
1 mm/min; ASTM D638
LG Chemical HT700 ABS, High Stiffness
Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
Tensile Modulus 2.39 GPa
346 ksi
ASTM D-638
Axiall 9246 Rigid PVC, Molding
Georgia Gulf 9246 is a high impact compound suitable for food packaging.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.