Mechanical Properties Metric English Comments
Tensile Modulus 23.3 GPa
3380 ksi
ASTM D638
LNP Thermocomp® EC-1006 EM Polyetherimide, Carbon Fiber Reinforcement  (discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
Tensile Modulus 23.3 GPa
3380 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® FC -1160 Polyphthalamide (PPA), 60% Glass Fiber
Amodel® FC-1160 is an FDA-approved, 60% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h..
Tensile Modulus 23.3 GPa
3380 ksi
1 mm/min, Type 1A; ISO 527-2
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621..
Tensile Modulus 23.3 GPa
3380 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP EC006E PEI
LNP THERMOCOMP* EC006E is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive
Tensile Modulus 23.3 GPa
3380 ksi
ISO 527-2/1A/1
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr..