Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.32 GPa | 337 ksi | ASTM D-638 |
Axiall Suprel® SVA 9812 Rigid PVC, Extrusion Georgia Gulf Suprel® SVA 9812 Alloy is an extrusion grade thermoplastic designed for sheet or profile applications requiring high impact resistance. Key features of Suprel 9812 alloy are flame ret.. |