Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 33.33 GPa | 4834 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON RE008 PA 66 LNP* STAT-KON* RE008 is a compound based on Nylon 66 containing 40% Carbon Fiber. Characteristics of this grade include: Electrically Conductive. |