Mechanical Properties Metric English Comments
Tensile Modulus 32.44 GPa
4705 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Stat-kon REL36 PA 66
LNP* Stat-Kon* REL36 is a compound based on Nylon 6/6 containing carbon fiber and PTFE. Characteristics of this grade are Statically Conductive.This data was supplied by SABIC-IP for the Americas r..