Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 31.03 GPa | 4501 ksi | ASTM D-638 |
PlastiComp Velocity® LCF40-PA66 High Flow Nylon 66, 40% Long Carbon Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |