Tensile Modulus 2.119 GPa

@Temperature -40.0 °C
307.3 ksi

@Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612  (Unverified Data**)
Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers