Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 30.42 GPa | 4412 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP ECL36XXQ PEI LNP* Lubricomp* ECL36XXQ is a compound based on Polyetherimide containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |