Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 30.08 GPa | 4363 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF008S PA 66 LNP* THERMOCOMP* RF008S is a compound based on Nylon 6/6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 30.08 GPa | 4363 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RX05494 PA 66 LNP* Thermocomp* RX05494 is a compound based on Nylon 6/6 resin containing glass fiber fillers. Added features of this material include: Heat Stabilized. |