Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.71 GPa | 538 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RX05487 PA 66 LNP* LUBRICOMP* RX05487 is a compound based on Nylon 66 containing 10% Aramid Fiber, 10% Lubricant. Added features of this material are: Low Warpage, Wear Resistant. |
|||
Tensile Modulus | 3.71 GPa | 538 ksi | Storage |
Epoxy Technology EPO-TEK® 320NC Optically Opaque Epoxy Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Tensile Modulus | 3.71 GPa @Temperature 120 °C |
538 ksi @Temperature 248 °F |
ISO Data |
BASF Petra® 130 FR BK-112 30% Glass Filled PET Petra 130 FR BK-112 is a 30% glass fiber reinforced, black pigmented, flame retardant injection molding compound based on post-consumer and post-industrial recycle polyethylene erephthalate feedstoc.. |