Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.69 GPa | 535 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON EX01696C PEI LNP* STAT-KON* EX01696C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Tensile Modulus | 3.69 GPa | 535 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON EX01696C PEI (Asia Pacific) LNP* Stat-kon* EX01696C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |