Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0245 GPa | 3.55 ksi | |
Zeon Chemicals Zetpol® ZCS 2395 Hydrogenated Nitrile Elastomomer Zeoforte® ZSC 2395 is a highly saturated copolymer of butadiene and acrylonitrile, which has been modified with the zinc salt of methacrylic acid. ZSC 2395 has excellent physical properties and a.. |