Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0241 GPa | 3.50 ksi | ASTM D638 |
3M Dyneon™ CC646/S Custom Compound
(discontinued **) This compound consists of a mixture of 60% bronze blended with PTFE.Information provided by Dyneon, A 3M Company |