Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.49 GPa | 506 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DD0001I PC LNP* STAT-KON* DD0001I is a compound based on Polycarbonate resin containing Carbon Powder. Added features include: ECO FR rating of 94V-0 @ 3.0mm and 94V-1 @ 1.5mm, High Impact. |
|||
Tensile Modulus | 3.49 GPa | 506 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 3.49 GPa | 506 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Asia Pacific) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 3.49 GPa | 506 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Europe-Africa-Middle East) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |