Polymer Property : Tensile Modulus = 3.321 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.628 - 3.321 GPa
381.2 - 481.7 ksi
ASTM D638
3D Systems Accura® 40 Plastic for SLA® Systems
40 Accura "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsHigh temperature testing:Automotive "under-the-hood" partsIntake manifoldsLighting components a..