Polymer Property : Tensile Modulus = 3.02 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.02 GPa
438 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Lubricomp CI001 PS
LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the America..
Tensile Modulus 3.02 GPa
438 ksi
Molded; ASTM D882
Honeywell Aegisâ„¢ H155MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H155MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
Tensile Modulus 3.02 GPa
438 ksi
1 mm/min
Arkema Group Nakan® RPS 400 M PVC, Rigid Extrusion Grade
NAKAN RPS 400 M is a rigid polyvinyl chloride compound developed for extrusion of cables ducts.ISO data provided by the manufacturer, Arkema.
Tensile Modulus 3.02 GPa
438 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Lubricomp CI001 PS (Asia Pacific)
LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pa..