Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 20.64 GPa | 2994 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP WCL36 PBT LNP* LUBRICOMP* WCL36 is a compound based on PBT resin containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant. |