Mechanical Properties Metric English Comments
Tensile Modulus 20.07 GPa
2911 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP IF00C PA6.12
LNP* THERMOCOMP* IF00C is a compound based on Nylon 6/12 resin containing 60% Glass Fiber.