Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 290 GPa | 42000 ksi | |
Toho Tenax Besfight® G40-600 12K IMA-7C EP03 Continuous Filament Carbon Fiber Intermediate Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho.. |